CuSn6P
Phosphor Bronze
Chemical Composition (%) |
|||||||||||||
Standard |
Class |
Alloy |
Cu |
Al |
Fe |
Mn |
Ni |
P |
Pb |
Si |
Sn |
Zn |
Other |
ISO24373 |
Cu5180 |
CuSn5P |
bal. |
0.01 |
- |
- |
- |
0.1- 0.4 |
0.02 |
- |
4.0- 6.0 |
- |
0.5 |
GB/T9460 |
SCu5180 |
CuSn5P |
bal. |
max 0.01 |
- |
- |
- |
0.1- 0.4 |
max 0.02 |
- |
4.0- 6.0 |
- |
max 0.5 |
ISO24373 |
Cu5180A |
CuSn6P |
bal. |
0.01 |
0.1 |
- |
- |
0.1- 0.4 |
0.02 |
- |
4.0- 7.0 |
0.1 |
0.2 |
GB/T9460 |
SCu5180A |
CuSn6P |
bal. |
max 0.01 |
max 0.1 |
- |
- |
0.01- 0.4 |
max 0.02 |
- |
4.0- 7.0 |
max 0.1 |
max 0.2 |
BS EN14640 |
Cu5180 |
CuSn6P |
bal. |
0.01 |
0.1 |
- |
- |
0.1- 0.4 |
0.02 |
- |
4.0-7.0 |
0.1 |
0.40 |
AWS A5.7 |
C51800 |
ERCuSn-A |
bal. |
0.01 |
- |
- |
- |
0.10- 0.35 |
0.02 |
- |
4.0-6.0 |
- |
0.50 |
DIN 1733 |
2.1022 |
SG-CuSn6 |
bal. |
max 0.01 |
max 0.1 |
- |
- |
0.01- 0.35 |
max 0.02 |
- |
5.0-8.0 |
max 0.1 |
max 0.4 |
Physical Properties And Mechanical Properties:
Solids-Temperature |
910℃ |
Liquids-Temperature |
1040℃ |
Density |
8.7㎏/ dm3 |
TensileStrength |
320~360 N/ mm2 |
Elongation |
20~25% |
Brinell Hardness |
80~90HB |
Introduction
Particularly suitable for the welding of copper with Cu-Sn alloy, especially for the butt joining welding of brass with steel. Can also be used in repairing cast copper product. Pre-heat suggested for large size products, and pulsed argon arc welding is recommended for multilayer hard facing on steel.