CuSn9P
Phosphor Bronze
Chemical Composition(%) |
|||||||||||||
Standard |
Class |
Alloy |
Cu |
Al |
Fe |
Mn |
Ni |
P |
Pb |
Si |
Sn |
Zn |
Other |
ISO24373 |
Cu5210 |
CuSn8P |
bal. |
- |
0.1 |
- |
0.2 |
0.01-0.4 |
0.02 |
- |
7.5-8.5 |
0.2 |
0.2 |
GB/T9460 |
SCu5210 |
CuSn8P |
bal. |
- |
max 0.1 |
- |
max 0.2 |
0.01-0.4 |
max 0.02 |
- |
7.5-8.5 |
max 0.2 |
max 0.2 |
BS EN14640 |
Cu5210 |
CuSn9P |
bal. |
- |
0.1 |
- |
- |
0.01-0.4 |
0.02 |
- |
7.0-9.0 |
0.2 |
0.5 |
AWS A5.7 |
C52100 |
ERCuSn-C |
bal. |
0.01 |
0.10 |
- |
- |
0.10-0.35 |
0.02 |
- |
7.0-9.0 |
0.20 |
0.50 |
Physical Properties And Mechanical Properties:
Solids-Temperature |
875℃ |
Liquids-Temperature |
1025℃ |
Density |
8.8㎏/ dm3 |
TensileStrength |
260 N/ mm2 |
Elongation |
20% |
Brinell Hardness |
80HB |
Introduction
Recommended for the welding of copper with Cu-Sn alloy. Best for the butt joining welding of brass with steel. Pre-heat suggested for the large size products, and pulsed argon arc welding is recommended for multilayer hard facing on steel.